Molybdenum dioxide is deposited on the form of an aerogel (in the autoclave) on nickel Mond. The catalytic activity for the hydrogenation of benzene into cyclohexane at 100°C depends on the proportion of MoO2 and on the temperature of a pretreatment in hydrogen. When this temperature is 440°C, the catalytic activity exceeds that of pure nickel Mond and exhibits a maximum for about 10% of MoO2. This synergetic effect, which is an exemple of a strong metal-support interaction (SMSI), is explained by the incorporation into the surface of nickel Mond crystals of molybdenum produced by partial reduction of MoO2, with the formation of an inter-metallic compound MoNi4. On depose du bioxyde de molybdene, sous forme d'aerogel (dans l'autoclave), sur du nickel de Mond. L'activite catalytique pour l'hydrogenation du benzene en cyclohexane, a 100°C, depend de la proportion de MoO2 et de la temperature d'un pretraitement dans l'hydrogene. Quand cette temperature est de 440°C, l'activite catalytique excede celle du nickel de Mond pur et elle atteint un maximum lorsque la teneur en MoO2 est d'environ 10%. Cet effet synergetique, qui est un exemple d'une forte interaction metal-support (SMSI), s'explique par l'incorporation, dans la surface des cristaux de nickel de Mond, du molybdene produit par reduction partielle de MoO2, avec formation de MoNi4, un compose intermetallique.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    11
    References
    9
    Citations
    NaN
    KQI
    []