Influence of the pulse duration at near-infrared wavelengths on the laser-induced material removal of hot-dipped galvanized steel

2020 
Hot-dipped galvanized steel is processed with short- and ultrashort-pulsed lasers in air at near-infrared wavelengths with pulse durations ranging from 350 fs to 241 ns. The morphology of the ablat...