Shear bond strength of veneering porcelain to porous zirconia

2014 
: In this study, two types of porous zirconia and dense zirconia were used. The flexural strength of non-layered zirconia specimens and those of the layered zirconia specimens with veneering porcelain were examined. Furthermore, the shear bond strength of veneering porcelain to zirconia was examined. The flexural strength of the non-layered specimens was 1,220 MPa for dense zirconia and 220 to 306 MPa for porous zirconia. The flexural strength of the layered specimens was 360 MPa for dense zirconia and 132 to 156 MPa for porous zirconia, when a load was applied to the porcelain side. The shear bond strength of porcelain veneered to dense zirconia was 27.4 MPa and that of porcelain veneered to porous zirconia was 33.6 to 35.1 MPa. This suggests that the veneering porcelain bonded strongly to porous zirconia although porous zirconia has a lower flexural strength than dense zirconia.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    25
    References
    6
    Citations
    NaN
    KQI
    []