Abstract Objectives The purpose of this study was to identify the combination of orthodontic adhesive resins and light-emitting diode (LED) light-curing units (LCUs) that result in the highest degree of resin conversion (DC). The hypothesis tested was that pairing orthodontic resins with LCUs from the same manufacturer produces higher DC versus unpaired resins and LCUs. Methods Pre-polymerization spectra of adhesive resins (Transbond XT [3M Unitek], BracePaste [American Orthodontics] or Opal Bond MV [Opal by Ultradent]) were obtained at oral temperature (37°C) using an attenuated total reflectance (ATR) diamond crystal (Golden Gate, Specac) in a Fourier-transform infrared (FTIR) spectrometer (Nicolet IS50). Resin specimens were polymerized using various LCUs (Ortholux Luminous [3M Unitek], Blue Ray 3 [American Orthodontics], or VALO Ortho Cordless [Ultradent Products, Inc.]) before obtaining post-polymerization infrared (IR); spectra. Twelve LCU-resin combinations were tested (n = 20/combination), half with a bracket present (Mini Diamond Twin, Ormco) and half without. DC values (%) were calculated using the two-frequency method and tangent-baseline technique. Data for each resin were statistically analyzed using General Linear Models and Student-Newman-Keuls post hoc tests (α = 0.05). Results Statistically significant differences were found within each resin for the groups without brackets present (P Conclusions Adhesive resins and LCUs from the same manufacturer did not consistently result in statistically higher mean DC values than unpaired combinations. Metal brackets do not uniformly reduce the degree of conversion of adhesive resins when assessed using IR spectrometry.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    23
    References
    0
    Citations
    NaN
    KQI
    []