Interfacial structure and joint strength on Ti(C, N)–Al2O3 cermet/40Cr steel joints with diffusion bonding

2019 
The Ti(C, N)–Al2O3 cermet to 40Cr steel joint was conducted by liquid phase diffusion bonding under the auxiliary pulse current and using 73Cu–27Ti amorphous foil/Cu foil/72Ag–28Cu foil sandwich fo...