Deposition of antimony sulfide thin films from single-source antimony thiolate precursors

2007 
Antimony sulfide thin films have been deposited for the first time by MOCVD using antimony thiolates Sb(SR)3 (R = But (1), CH2CF3 (2)) as single-source precursors. The structure of 1 was determined by X-ray crystallography and shown to be a monomer. Films were grown from 1 and 2 by low-pressure CVD using both glass slides and silicon wafers as substrates, at substrate temperatures of 300 and 450 °C, respectively. In both cases, the deposited films exhibited XRD patterns that could be fully indexed to orthorhombic stibnite, with stoichiometries in the range Sb2S2.78-3.10 by EDXS. In addition, there is evidence for the formation of small amounts of antimony metal in the films derived from 2. The morphologies of the films are strongly substrate dependent:  1 generates random platelets regardless of substrate, whereas 2 deposits a uniform film with islands of needle morphology on glass or long rods of stacked platelets on Si. A film deposited on glass is photoactive and has a band gap of 1.6 eV.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    40
    References
    25
    Citations
    NaN
    KQI
    []