국산 유용 수종의 오일열처리 연구 I

2015 
Among several thermal wood modification methods German oil heating technology was applied for color changing larch and paulowniawood specimens. They were heat treated at 200°C for 3 hours in an autoclave filled with linseed oil. The CIE L*a*b* color indexes of the shells and cores of the oil heated specimens were measured. The color difference indexes between the oil heated and the control specimens of larch and paulowniawood were in the range of 6 and 12, which implies considerably different. The color difference indexes between the core layers of the larch and paulowniawood specimens were 4.3 and 1.7, respectively. It could be concluded that the specimens of the two species were color changed uniformly by oil heating.