2016 
A kind of method for reducing cold-rolled biphase steel aberration is the embodiment of the invention provides, for reducing cold-rolled biphase steel surface chromatic aberration.Methods described includes:According to required Cold Rolled Plate Thickness, hot rolling plate thickness is determined;According to the hot rolling plate thickness, hot rolling is carried out to slab by hot rolling mill, obtain hot rolled plate;The hot rolled plate is cooled down in layer cool equipment, and temperature-compensating is carried out at least a portion in the hot head and hot tail of the hot rolled plate;The hot rolled plate is coiled into strip in coiling machine.