Influence of starting powder choice on structure property relations in gadolinia stabilized zirconia 3Gd-TZP manufactured from co-milled starting powders

2021 
Abstract Two 3Gd-TZP materials were manufactured from powders produced by intense mixing and milling of unstabilized zirconia starting powders and gadolinia as stabilizer oxide by hot pressing at 1250 °C – 1400 °C. The materials show a combination of high toughness and moderate strength. In detail depending on starting powder the two TZP showed distinct differences concerning transformation characteristics, sintering temperature dependence of mechanical properties and the tendency to develop R-curve related deformation features such as non-linear stress strain curves and formation of transformation bands prior to fracture.