Ultra-SAXS observation of fibril-sized structure formation after the necking of poly(ethylene terephthalate) and poly(phenylene sulfide) fibers

2019 
Fibril-sized structures, which exhibit a density fluctuation of several tens to hundreds of nanometers, are important because they influence many properties of fibers and films, particularly the strength and thermal shrinkage of synthetic fibers. We analyzed the formation of fibril-sized structures after necking using ultra-small-angle X-ray scattering (USAXS), which enables observation of the void and craze formations. Continuous laser-heated drawing and undulator synchrotron radiation were adopted to measure the structural development of poly(ethylene terephthalate) (PET) and poly(phenylene sulfide) (PPS) fibers. Both fibers showed a clear increase in the meridional streak intensity just after necking and an increase in the equatorial streak after necking. These increases were distinctive for PPS. Moreover, a layer-lined streak appeared after necking only for PET. The intensity of the meridional streak increased with an increase in the draw ratio, whereas the intensity of the layer-lined scattering decreased with an increase in the draw ratio.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    23
    References
    2
    Citations
    NaN
    KQI
    []