Shear Bond Strength of Different MDP-Containing Adhesive Systems on Enamel and Dentin from Primary Teeth.

2021 
Objective To compare the shear bond strength (SBS) after thermocycling of four universal adhesives applied in self-etch mode on dentin and etch-and-rinse mode on enamel. Study design Flat 144 buccal or lingual dentin and enamel surfaces from 72 non-carious primary molars were prepared. Samples were segregated into 12 groups (n=12): Adper Single Bond 2 etch-and-rinse (SB_T) and Clearfil SE Bond self-etch (SE_S) applied to enamel and dentin served as controls. Scotch Bond Universal Adhesive (SBU), Clearfil S3 Bond Universal Adhesive (SEU), Tetric N-Bond Universal Adhesive (TEN), and All Bond Universal (BIS) were applied in etch-and-rinse mode to enamel and in self-etch mode to dentin. They were thermocycled for 5000 cycles. SBS testing and the evaluation of fracture mode were performed. Results SB_T showed statistically higher SBS than other adhesive groups using etch-and-rinse mode on enamel. SE_S and BIS had statistically higher SBS than other adhesive groups using self-etch mode on dentin. Mixed failure was the most common failure mode in each group. Conclusion The universal adhesives did not show higher SBS than SB_T when using etch-and-rinse on enamel. All universal adhesives showed higher SBS than SB_T and had SBS similar to SE_S, except SBU when using self-etch mode on dentin.
    • Correction
    • Source
    • Cite
    • Save
    • Machine Reading By IdeaReader
    0
    References
    0
    Citations
    NaN
    KQI
    []