A simple and practicable evaporation-induced self-assembly (EISA) method is introduced for the first time to prepare nanosized solid electrolyte Li1.4Al0.4Ti1.6(PO4)3 (LATP) for all-solid-state lithium-ion batteries. A pure Na+ super ion conductor (NASICON) phase is confirmed by X-ray diffraction (XRD) analysis, and its primary particle size is down to 70 nm by optimizing evaporation rate of the solvent. Excellent room temperature bulk and total lithium-ion conductivities of 2.09 × 10−3 S cm−1 and 3.63 × 10−4 S cm−1 are obtained, with an ion-hopping activation energy as low as 0.286 eV.