Manipulation of K center charge states in silicon nitride films to achieve excellent surface passivation for silicon solar cells
2014
High quality surface passivation (Seff ±8 × 1012 cm−2) into a dual layer stack of Plasma Enhanced Chemical Vapor Deposition (PECVD) Silicon Nitride (SiNx)/PECVD Silicon Oxide (SiO2) films using a corona charging tool. We demonstrate long term stability and uniform charge distribution in the SiNx film by manipulating the charge on K center defects while negating the requirement of a high temperature thermal oxide step.