Predominance Area Diagrams Bounding the Cu-As-S-O System’s 3D Predominance Diagram at 900 K (627 °C)

2019 
The two-dimensional predominance area (Kellogg) diagram (PAD) surfaces bounding the three-dimensional Cu-As-S-O system were constructed at 900 K. The computations employed gases As4O6(g), O2(g), and SO2(g) as the independent coordinate species to generate diagrams of As4O6(g) − O2(g),O2(g) − SO2(g), and As4O6(g) − SO2(g), while the third gas (As4O6, O2, or SO2) was fixed. The results indicate that there is no shared boundary between enargite (Cu3AsS4) and copper sulfate (CuSO4); however, at \( {\mathrm{P}}_{{\mathrm{O}}_2} {10}^{-4} \) atm, CuSO4 is the stable phase at 900 K. The chemical driving force for oxidation of intermediate phases between enargite and copper sulfate is substantial except for basic sulfate (CuO · CuSO4).