Preparation and Properties of Solid Electrolyte CaxBi1.7-xW0.3O3.45-0.5x Electrolyte Material by Sol-Gel Combution Method
2019
CaxBi1.7−xW0.3O3.45−0.5x (CBW) (x=0.00, 0.05, 0.10, 0.15, 0.20, 0.30) electrolyte material were synthesized by sol–gel self-combustion method. The samples were characterized by thermogravimetric-di...