The thermodynamic analysis and tests of minerogenesis under higher temperatures determine conditions of thermochemical decomposition of hydrophilic attachments on diamond surface. It is found that hydrophilic mineral attachments can be removed from diamond surface by combining thermal treatment of slurry at the temperature of 80–85  $$^\circ$$ C with electrochemical treatment of recirculated water, which enables required change in ion–molecule composition of water phase in the slurry. The hybrid conditioning technology ensures recovery of the natural hydrophobic behavior and floatability of diamonds and enhances performance of froth flotation of diamonds by 5.1%.